Used as 5-10% aqueous emulsion in the processing of metals by cutting and pressure, at the cold rolled stage of carbon and alloy steels, oiling the steel tape before wrapping it in a roll.
The most suitable water for emulsion preparation has hardness up to 6 mg·eq/ dm³, without coarsely dispersed impurities and chemical additives.
Before the aqueous emulsion preparation, the concentrate of the agent is thoroughly mixed in a storage container. The estimated quantity of the agent is loaded in the container equiped with a mixer. Than, water (15-45°C) is supplied in small portions or a thin steam with constant stirring.
After water loaded, the mixture is thoroughly mixing until a homogeneous emulsion has formed.